Free shipping on all orders over $50
7-15 days international
25 people viewing this product right now!
30-day free returns
Secure checkout
80166173
Bambu ASA is a highly durable material that offers exceptional UV, weather, mechanical, and thermal resistance. Its unique combination of properties makes it an ideal material for printing outdoor models (plant signs, mailboxes, wind vanes, etc.) and structural parts that require long-term exposure to challenging outdoor conditions.
Bambu ASA offers extraordinary UV, oxidation, and aging resistance, providing effective protection against breakage and color degradation when used outdoors for long-term purposes.
Suitable for outdoor applications and regular structural requirements due to its toughness and high impact strength.
Compared to normal PETG or ABS, Bambu ASA can remain in shape even at a temperature of 100°C.
ABS | ASA | |
Composition | acrylonitrile - butadiene - styrene | acrylonitrile - styrene - acrylate |
ASA is a modified version of ABS that contains an additional acrylate component, which improves its weather adaptability and UV resistance.
ASA retains the impact resistance and processability of ABS while providing better resistance to fading, yellowing, and degradation from sunlight exposure. Both of them may release pungent and unpleasant odors during printing, but the pungent odor of ASA is notably lighter than ABS.
ASA is ideal for outdoor applications, such as automotive exterior parts, signage, and outdoor equipment, thanks to its enhanced weather resistance and color stability. ABS is a versatile material with excellent mechanical properties that is commonly used for indoor applications.
In terms of physical and mechanical properties, both exhibit good impact resistance and high tensile strength, with almost the same levels of strength, toughness, and stiffness. Both ABS and ASA may release pungent and unpleasant odors during printing and require the same enclosed printer settings when printing large-size and/or high-infill dense models.
Recommended | Not Recommended | |
Build Plate | Engineering Plate, High Temperature Plate or Textured PEI Plate | Cool Plate |
Hotend | All Size / Material | / |
Glue | Bambu Liquid Glue Glue Stick | / |
All printing parameters are embedded in RFID, which can be read through our AMS (Automatic Material System).
Load and print! No more tedious setting steps.
Drying Settings before Printing | 80 °C,8 h |
Printing and Keeping Container's Humidity | < 20% RH (Sealed, with Desiccant) |
Nozzle Temperature | 240 - 270 °C |
Bed Temperature (with Glue) | 80 - 100 °C |
Printing Speed | < 250 mm/s |
Density | 1.05 g/cm³ |
Vicar Softening Temperature | 106 °C |
Heat Deflection Temperature | 100 °C |
Melting Temperature | 210 °C |
Melt Index | 7.0 ± 0.8 g/10 min |
Tensile Strength | 52 ± 5 MPa |
Breaking Elongation Rate | 9.2 ± 1.4 % |
Bending Modulus | 1920 ± 130 MPa |
Bending Strength | 74 ± 4 MPa |
Impact Strength | 41.0 ± 2.3 kJ/m² |
• Pungent and unpleasant odors may be released during printing. Make sure your printer is placed in a well-ventilated area.
• ASA is prone to warping when printing large size and/or high infill density model. To avoid warping: 1) Use enclosure printers and ensure the build plate is properly glued before printing. 2) Set lower printing speed or higher heatbed temperature.
• Recommended to dry out before use to get higher printing quality.